Reason steel welding crack and Prevention

Time:[2016-2-20]  Hits:4268

Guangzhou Steel tells you: Reason steel welding crack and Prevention

 

(A) hot cracking
Hot cracking refers to crack under high temperatures generated, also known as high-temperature cracks or solidification cracking, usually generated internally welds may sometimes occur in the heat affected zone, manifestations are: longitudinal cracks, transverse cracks, root crack crater cracks and heat-affected zone cracking. Its causes is due to the existence of the weld puddle segregation during crystallization, a low melting point eutectic and impurities in the crystallization process in the form of a liquid layer between the presence of segregation to form a solidified after a lower intensity, welding stress is large enough when , they will be among just solidified liquid layer or near-solid metal opened a crack. In addition, if the grain boundaries of the base material there is also a low melting point eutectic and impurities, when welding the tensile stress is large enough, it will also be opened. In short, the thermal cracking is the result of metallurgical factors and mechanical factors working together. For its causes, and its prevention measures are as follows:
(1) limit the base metal and welding materials (including rod, wire, flux and shielding gas) easily segregation element content and harmful impurities, in particular, shall control the sulfur and phosphorus content and lower carbon content, generally used for welding in steel sulfur content should not exceed 0.04 5% phosphorus content should not exceed 0.055%; in addition the carbon content of the steel from the welding performance worse, general weld carbon content of 0.10% or less in control, thermal cracking susceptibility It can be greatly reduced. (2) to adjust the chemical composition of the weld metal to improve weld, the weld refined grain products to increase its plasticity, or reduce the degree of dispersion of segregation, control the harmful effects of a low melting point eutectic. (3) using basic electrodes or flux to reduce the weld containing impurities taken to improve the degree of crystallization of segregation. (4) an appropriate increase in the shape factor of the weld, using multi-pass welding method avoids the centerline segregation prevented centerline cracks. (5) the use of reasonable welding sequence and direction, a smaller weld lines can be super, overall warm-up and hammering method, fill the crater at Crater other process measures.
(B) cold cracking
Generally refers to the weld cold cracking during cooling down to the martensite transformation temperature of the temperature range (hereinafter 300-200 ℃) produced, can occur immediately after welding, it can also occur in a long time after the welding, it is also called delayed cracking. There are basic conditions for the formation of 3: welded joint forming hardened tissue; the presence and concentration of hydrogen diffusion; and there is a large welding tensile stress. Its preventive measures are:
(1) Guangzhou steel welding specifications and choose the right line can improve the weld metal and heat affected zone state organizations, such as preheating before welding, interlayer temperature control, slow cooling after welding or the like to accelerate the hot hydrogen molecules escape . (2) using basic electrodes or flux to reduce the oxygen content in the weld diffusion. (3) electrode and flux before use should be strictly in accordance with the requirements for drying (low hydrogen electrodes 300 ℃ ~ 3 50 ℃ incubated lh; acid electrode l 00 ℃ ~ l50 ℃ incubated lh; solder 200 ℃ ~ 250.C insulation 2h), carefully cleaning the groove and the wire, so in addition to oil, water and dirt, rust, etc., in order to reduce the source of hydrogen. (4) timely post-weld heat treatment. First, an annealing treatment to eliminate stress, so that quenching and tempering to improve their toughness; two: eliminate the hydrogen treatment is carried out, the hydrogen from the weld joint fully escape. (5) improve the quality of steel, reducing the steel layered inclusions. (6) can be taken to reduce stress in a variety of welding process measures.

Copyright:佛山市胜邦钢结构有限公司 Foshan Shengbang Steel Structure Co., Ltd. Record Number:粤ICP备13078463号
AVENTICS气动阀| 机械剥离专用蓝膜| 有机垃圾处理设备| 蒸汽平板硫化机| 绳式高压验电器| NICHIBAN米其邦胶带| 沥青动力粘度试验器| 钢板切割加工「厂家价格低」| 非接触光学表面测量| 发格伺服电机维修| 中水回用| 恒温房| 埃福创AVTRON编码器| 查特MVE液氮罐| 套筒补偿器| 无菌全自动封管机| 纸张撕裂度仪| 氯化锂蒸发浓缩器| 复合土工膜| 试验变压器| 长沙路基板租赁| MiltonRoy米顿罗电磁泵| 动物疼痛测量仪| 西林叉车| elisa试剂盒供应厂商| 超声电动显微分析系统| PARKER电磁阀| 高纯氩分析色谱| 重介质旋流器维修| 瑞士Borer清洗液| 蓝牙音频分析仪| PDS863液位变送器| 北斗定位终端与GPS卫星导航设备生产厂家| 个人剂量报警仪| 昆山欣鹏盛五金机械| 非接触膜厚仪| 无损探伤设备网| 船用真空马桶(排放阀| 三相数显电压表| 通用绝缘电阻测试仪| 总锡|