How to prevent corrosion of building steel structure?

Time:[2022-1-11]  Hits:1983

Under normal circumstances, the steel structure does not corrode or corrodes slowly after adding a protective layer. The life of some buildings can reach hundreds of years, but under some conditions, the steel structure has an amazing corrosion rate, which can be rusted in a few years or less. Destruction of buildings can be done within a short period of time. The corrosion process is generally as follows: micro-cracks and holes in the protective layer of the steel structure, peeling of the protective layer, intrusion of harmful media; corrosion of the steel structure; severe corrosion of the steel structure; reduction of the performance of the steel structure and damage to the structure or components. Its anti-corrosion treatment can generally be considered from two aspects:

a.Take measures according to the corrosion level

The corrosion of building steel structure can be divided into four grades: strong, medium, weak, and no. Under the condition of strong rust (a large amount of CO2, SiO2, H2S industrial environment), the corrosion rate of the material is fast, and the components and parts must be protected by surface isolation; under the condition of moderate rust, the material has a certain degree of rust, and the weight of the component can be increased. , or use simple surface protection; under weak rust conditions, the material rusts slowly, but some measures need to be taken; under no rust conditions, the material rusts very slowly or there is no obvious rust trace, and components and parts may not take protective measures.

b.Processing of key links

Base treatment: The anti-corrosion base treatment of the steel structure should be qualified and meet the specific requirements of the design drawings, such as the use of alkyd paint, epoxy zinc-rich paint, galvanized, etc.

Temperature and humidity: The ambient temperature and relative humidity during coating should meet the product requirements, the ambient temperature should be 5-38°C, the relative humidity should not be greater than 85%, and the surface should not be coated with dew. Do not rain within 4 hours after painting.

Thickness of spray coating: It should meet the design requirements, and the spray coating used on the day should be configured on the same day, and operate according to the anti-rust spray coating operation specifications. Coating performance: The influence of various harmful media on the steel structure should be considered, and the spray coating suitable for the working environment should be selected to ensure the anti-corrosion quality.

Copyright:佛山市胜邦钢结构有限公司 Foshan Shengbang Steel Structure Co., Ltd. Record Number:粤ICP备13078463号
过滤洗涤干燥三合一| 摩擦系数测试仪| 无锡网站建设| 免疫球蛋白国际标准品| 高压消杀设备| 塑料色母粒厂家| 潜水员水下封堵施工| 气动潜水推流器| 邯郸便道砖| DF| 内窥镜图像处理器| 环氧玻璃丝管| 固废处理设备厂家| 微量氧气分析仪| 检测| 威海珍珠棉厂家| 凸鼻数显洛式硬度计| 鉴定试剂盒| 地埋电线故障查找设备| 钢筋位置测定仪| 电子温度开关| 光纤压力传感器| 皮带输送机| 双动力锯齿波跳汰机| pe耐磨板| 淄博工地拉丝门套线| 众诺财税| 边压环压试验机| 复合钢格板| 带打网孔拉伸膜| 进口粘度计| 气力提升泵| 常州市国立试验设备研究所| 精密孔加工| 伺服编码器电缆| 人乳腺癌细胞MCF| 葵花籽脱壳机组| 低温水浴恒温振荡器| 斗式提升机厂家| 蒸发浓缩赶酸仪| Julabo粘度计|